Main Product Super Bright Expansion Alloy 1J33/ 4J29/4J33/Invar 36 Wire Precision Alloy wire

Categories Precision Alloy
Brand Name: Victory
Model Number: Permalloy 80
Place of Origin: China
MOQ: 50
Price: $25-$40
Payment Terms: L/C, T/T, Western Union, MoneyGram
Supply Ability: 200 tons per month
Delivery Time: 5-21 days
Packaging Details: Standard Export Wooden Cases Ex.Gross Weight Under 20kg=Carton Box/Gross Weight over 20 kg=Plywood Box Or as per Request
Material:: NiFe
Certificate: ISO9001
Shape: wire, strip, foil, sheet
Resistivity:: 0.56
density:: 8.75g/cm3
size: customized
Standard:: GB/ASTM/AISI/ASME
Condition:: Bright, Annealed, Soft
Application:: Industrial Magnet
Curie Point:: 400℃
HCR:: 30
Feature:: high initial permeability
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Main Product Super Bright Expansion Alloy 1J33/ 4J29/4J33/Invar 36 Wire Precision Alloy wire

High Permeability Soft Magnetic Alloy




Soft magnetic materials are utilized in two key areas - energy conversion and information processing. In the power industry, these materials are primarily used in high magnetic fields that have a high magnetic induction and low core loss of the alloy. On the other hand, in the electronics industry, these materials are mainly used in low or medium alloys that have a high magnetic permeability and low coercive force.


However, soft magnetic materials are not without their drawbacks. Due to the alternating magnetic eddy currents that are induced inside the material, there is a resultant loss. The smaller the resistance of the alloy, the greater the thickness, and the higher the frequency of the alternating magnetic field, the greater the eddy current losses and the more reduced the magnetic field becomes. To combat this issue, the material must be made thinner into a sheet or tape and then coated with an insulating layer. Alternatively, certain methods can be used to form an oxide insulating layer on the surface of the alloy. One commonly used coating for this purpose is magnesium oxide electrophoresis.


Iron-nickel alloys are often used in alternating magnetic fields, mainly for yoke iron, relays, small power transformers, and magnetically shielded components. Soft magnetic materials play a crucial role in energy conversion and information processing, making them an essential component in various industries.


Applications

High sensitivity and small power transformers, magnetic amplifiers, relays, chokes, magnetic heads for magnetic recording devices, magnetic shields, various tape wound cores, cut cores, and laminated cores used in weak magnetic fields.


MaterialCPSMnSiNiCrCoMoCuFe
Max
Permalloy800.030.0200.0200.3-0.60.15-0.3079.0-81.0--4.8-5.2≤0.2.Rest

rialShapeClassThickness or Diameter mmMagnetic permeability in 0.08A/m magnetic field intensity μ0.4(mH/m)Maximum permeability μm(mH/m)Coercivity(under saturation magnetic induction)Hc/A·m-1Saturation magnetic induction Bs/T
not less thanno greater than
Permalloy80Cold rolled strip0.03-0.0418000(22.5)80000(100)3.60.70
0.05-0.0928000(35)110000(137.5)2.40.70
0.10-0.1930000(37.5)150000(187.5)1.60.70
0.20-0.3440000(50)180000(225)1.20.70
0.35-1.0050000(62.5)250000(312.5)0.80.70
1.10-2.5040000(50)150000(187.5)1.20.70
0.03-0.0430000(37.5)110000(137.5)2.40.70
0.05-0.0940000(50)140000(175)1.60.70
0.10-0.1950000(62.5)180000(225)1.20.70
0.20-0.3460000(75)200000(250)1.00.70
0.3555040(68.8)260000(325)0.70.70
Hot rolled tape4.5-2030000(37.5)100000(125)1.60.70
Hot forged bar20-10030000(37.5)100000(125)1.60.70

MaterialShapeClassThickness or Diameter mmMagnetic permeability in 0.08A/m magnetic field intensity μ0.4(mH/m)Maximum permeability μm(mH/m)Coercivity(under saturation magnetic induction)Hc/A·m-1Saturation magnetic induction Bs/T
not less thanno greater than
Permalloy80Cold rolled strip0.03-0.0418000(22.5)80000(100)3.60.70
0.05-0.0928000(35)110000(137.5)2.40.70
0.10-0.1930000(37.5)150000(187.5)1.60.70
0.20-0.3440000(50)180000(225)1.20.70
0.35-1.0050000(62.5)250000(312.5)0.80.70
1.10-2.5040000(50)150000(187.5)1.20.70
0.03-0.0430000(37.5)110000(137.5)2.40.70
0.05-0.0940000(50)140000(175)1.60.70
0.10-0.1950000(62.5)180000(225)1.20.70
0.20-0.3460000(75)200000(250)1.00.70
0.3555040(68.8)260000(325)0.70.70
Hot rolled tape4.5-2030000(37.5)100000(125)1.60.70
Hot forged bar20-10030000(37.5)100000(125)1.60.70

Quality Main Product Super Bright Expansion Alloy 1J33/ 4J29/4J33/Invar 36 Wire Precision Alloy wire for sale
Send your message to this supplier
 
*From:
*To: Changzhou Victory Technology Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0